FERRIT EF KERNER

|
MODEL |
G.W |
STØRRELSE (mm) |
|||||
|
A |
B min |
C |
D |
E |
F |
||
|
EER26/19 |
12.4 |
25.5±0.6 |
19.8 |
7.5±0.3 |
7.5±0.3 |
6.6±0.3 |
9.5±0.3 |
|
EC28/20 |
25 |
28.5±0.5 |
21.8 |
9.9±0.3 |
11.4±0.3 |
6.0±0.2 |
10.0±0.2 |
|
EC28/28 |
33 |
28.5±0.5 |
21.8 |
9.9±0.3 |
11.4±0.3 |
10.0±0.2 |
14.0±0.2 |
|
EC28/34 |
36 |
28.5±0.5 |
21.8 |
9.9±0.3 |
11.4±0.3 |
13.0±0.2 |
17.0±0.2 |
|
EER29/16 |
31.2 |
29.8±0.5 |
22 |
9.5±0.3 |
9.5±0.3 |
11.4±0.2 |
16.0±0.2 |
|
EC29/28 |
33.6 |
29.4±0.6 |
22.3 |
9.9±0.3 |
11.4±0.3 |
10.0±0.2 |
14.0±0.2 |
|
EC29/34 |
37 |
29.4±0.5 |
22.3 |
9.9±0.3 |
11.4±0.3 |
13.0±0.2 |
17.0±0.2 |
|
EC32/24 |
48 |
31.8±0.5 |
26.6 |
13.2±0.2 |
20.2±0.3 |
9.2±0.2 |
12.0±0.2 |
|
ETD29/16 |
31.2 |
29.8±0.8 |
22 |
9.5±0.3 |
9.5±0.3 |
11.0±0.2 |
15.8±0.2 |
|
EC34/32 |
36.5 |
34.0±0.5 |
22 |
15.6±0.2 |
15.6±0.3 |
10.6±0.2 |
16.0±0.2 |
|
ETD34/35 |
44.4 |
34.2±0.8 |
25.6 |
10.8±0.3 |
10.8±0.3 |
12.3±0.3 |
17.5±0.3 |
|
ETD35/35 |
45 |
35.2±0.8 |
26.4 |
10.8±0.3 |
10.8±0.3 |
12.3±0.3 |
17.5±0.3 |
|
EC35/30 |
43.6 |
35.0±0.7 |
25.6 |
11.3±0.4 |
11.3±0.4 |
10.0±0.3 |
15.0±0.3 |
|
EC35/31 |
44 |
35.0±0.7 |
25.6 |
11.3±0.4 |
11.3±0.4 |
10.0±0.3 |
15.5±0.3 |
|
EC35/42 |
54 |
35.0±0.7 |
25.6 |
11.3±0.4 |
11.3±0.4 |
15.0±0.3 |
21.0±0.3 |
|
EC35/43 |
55 |
35.0±0.7 |
25.6 |
11.3±0.4 |
11.3±0.4 |
15.5±0.3 |
21.5±0.3 |
|
EC36/43 |
56.4 |
36.0±0.7 |
26.2 |
11.3±0.4 |
11.3±0.4 |
15.5±0.3 |
21.5±0.3 |
|
EC39/40 |
63 |
39.1±0.9 |
29.1 |
12.5±0.3 |
12.5±0.3 |
14.5±0.3 |
20.0±0.3 |
|
EC39/42 |
65 |
39.1±0.9 |
29.1 |
12.5±0.3 |
12.5±0.3 |
15.5±0.3 |
21.0±0.3 |
|
EC40/45 |
82 |
40.0±0.8 |
28.8 |
13.3±0.3 |
13.3±0.3 |
15.5±0.3 |
22.5±0.3 |
|
EER40/19/20 |
90 |
40.0±1.0 |
35.8 |
18.8±0.3 |
32.6±0.4 |
6.4±0.25 |
10.0±0.25 |
|
EC41/45 |
83 |
41.0±0.8 |
29.8 |
13.1±0.3 |
13.1±0.3 |
15.5±0.3 |
22.5±0.3 |
|
EC42/41/14.8 |
88 |
42.0±1.0 |
31.5 |
14.7±0.3 |
14.8±0.3 |
15.0±0.3 |
20.5±0.3 |
|
EC42/43/14.8 |
92 |
42.0±1.0 |
31.5 |
14.7±0.3 |
14.8±0.3 |
16.0±0.3 |
21.5±0.3 |
|
EC42/43/15.2 |
97.6 |
42.0±1.0 |
31.5 |
15.2±0.3 |
15.3±0.3 |
15.5±0.3 |
21.5±0.3 |
|
EC42/43/17.3 |
123 |
42.0±0.5 |
31.8 |
17.3±0.3 |
19.6±0.4 |
15.6±0.3 |
21.5±0.3 |
|
EC43/45/14.8 |
98 |
43.0±1.0 |
32.5 |
14.8±0.3 |
14.8±0.3 |
16.5±0.3 |
22.5±0.3 |
|
EC43/47 |
110 |
43.3±1.0 |
31.5 |
15.2±0.3 |
15.3±0.3 |
16.5±0.3 |
23.5±0.3 |
|
EC44/47 |
109 |
44.0±1.0 |
32.5 |
15.2±0.3 |
15.3±0.3 |
16.5±0.3 |
23.5±0.3 |
|
EC46/47 |
112 |
46.0±1.0 |
34 |
15.2±0.3 |
15.3±0.3 |
16.7±0.3 |
23.5±0.3 |
|
EC46/51 |
118 |
46.0±1.0 |
34 |
15.2±0.3 |
15.3±0.3 |
18.2±0.3 |
25.4±0.3 |
|
EC49/50 |
133 |
48.7±1.1 |
36.1 |
16.3±0.4 |
16.4±0.5 |
18.1±0.3 |
24.7±0.3 |
|
EC49.2/50 |
132 |
49.2±1.1 |
37.5 |
16.1±0.4 |
16.4±0.5 |
18.3±0.3 |
24.7±0.3 |
|
EC59/62 |
292 |
59.8±1.3 |
43.6 |
21.6±0.5 |
21.6±0.5 |
22.5±0.4 |
31.0±0.2 |
|
Model |
PARAMETER |
AL±25 %(nH/N^2) |
N.W(g) |
|||
|
C1mm-1 |
Lemm |
Aemm2 |
Vemm3 |
ZP40 |
||
|
EC26/19 |
1.14 |
48.9 |
43.0 |
2103 |
1900 |
10.5 |
|
EC28/20 |
0.57 |
48.2 |
84.5 |
4079 |
3800 |
27.2 |
|
EC28/28 |
0.76 |
64.2 |
83.8 |
5376 |
2850 |
29.0 |
|
EC28/34 |
0.91 |
76.1 |
83.4 |
6353 |
2400 |
31.2 |
|
EER29/16 |
0.94 |
72.0 |
76.0 |
5742 |
2200 |
28.5 |
|
EC29/28 |
0.78 |
65.4 |
83.7 |
5474 |
2800 |
29.3 |
|
EC29/34 |
0.92 |
77.3 |
83.6 |
6462 |
2400 |
31.5 |
|
EC32/24 |
0.45 |
59.8 |
132.8 |
7946 |
4800 |
42.2 |
|
ETD29 |
0.96 |
70.6 |
73.6 |
7640 |
2500 |
28.0 |
|
EC34/32 |
0.35 |
67.5 |
132.8 |
7946 |
6180 |
64.3 |
|
ETD34/35 |
0.82 |
79.0 |
97.0 |
7660 |
2750 |
41.0 |
|
ETD35/35 |
0.82 |
80.1 |
97.0 |
7780 |
2700 |
40.0 |
|
EC35/30 |
0.65 |
70.1 |
108.4 |
7595 |
3300 |
38.0 |
|
EC35/31 |
0.65 |
70.1 |
108.4 |
7595 |
3300 |
38.5 |
|
EC35/42 |
0.81 |
90.9 |
112.0 |
10100 |
2600 |
48.0 |
|
EC35/43 |
0.90 |
92.2 |
112.0 |
10320 |
2550 |
50.0 |
|
EC36/43 |
0.85 |
93.5 |
112.0 |
10470 |
2500 |
51.0 |
|
EC39/40 |
0.70 |
91.9 |
130.7 |
12012 |
3100 |
56.2 |
|
EC39/42 |
0.73 |
95.9 |
130.6 |
12529 |
3000 |
59.0 |
|
EC40/45 |
0.66 |
98.0 |
149.0 |
14600 |
3250 |
73.0 |
|
EER40/19/20 |
0.20 |
52.6 |
268.5 |
14150 |
11000 |
80.0 |
|
EC41/45 |
0.67 |
99.0 |
147.5 |
14620 |
3200 |
73.6 |
|
EC42/41/14.8 |
0.58 |
96.0 |
163.0 |
15660 |
3700 |
82.0 |
|
EC42/43/14.8 |
0.58 |
99.7 |
168.0 |
16617 |
3700 |
85.0 |
|
EC42/43/15.2 |
0.53 |
98.5 |
184.0 |
18142 |
4000 |
90.0 |
|
EC42/43/17.3 |
0.42 |
98.5 |
233.0 |
23000 |
5100 |
108.0 |
|
EC43/45 |
0.59 |
103.1 |
173.4 |
17883 |
3650 |
85.5 |
|
EC43/47 |
0.55 |
104.0 |
191.0 |
20044 |
4000 |
100.0 |
|
EC44/47 |
0.55 |
104.0 |
191.0 |
20044 |
4000 |
100.0 |
|
EC46/47 |
0.57 |
107.5 |
187.5 |
20150 |
4000 |
102.0 |
|
EC46/51 |
0.55 |
104.0 |
191.0 |
20044 |
4000 |
100.0 |
|
EC49/50 |
0.53 |
114.0 |
213.0 |
24200 |
4100 |
120.0 |
|
EC49.2/50 |
0.58 |
118.0 |
206.0 |
24490 |
3700 |
117.0 |
|
EC59/62 |
0.38 |
139.0 |
368.0 |
51500 |
5400 |
257.0 |
Populære tags: ferrit ec kerner, Kina ferrit ec kerner producenter, leverandører, fabrik